Hello Dale,
From what I've worked out the steel was test shot before the plate was fitted to the carriers, probably during manufacture whilst the plate was just flat, as I have seen test marks where it would be impossible to do once the hull was welded together.
Regards
Justin.
__________________
Go Kimi!
Met Gas LP2A carrier Hull no.2753-
Progressing slowly.
|