What is it in molasses that does the derusting...... the potassium content??? and if so would not a weak potassium acid bath be cheaper, faster, less sticky and stinky without being lethal to the environment?????
Bob, I believe molasses has a pH of around 5-6, which means it is acidic. I suspect it is the organic acids that are responsible for the de-rusting process. Since it is a relatively weak acid, it is not too destructive on the parts (as everyone has noted). Thats also why it takes a bit of time to produce results. If you go to a stronger solution, it may be faster but also more damaging to your sensitive parts.