Default Phosphoric Acid

Hi guys - when I finish electrolysis derusting I paint the metal with a dilute solution of this stuff. When dry it leave a white powder that I brush off, (mask required). This neutralises everything but etch priming must be done immediately as the red curse quickly starts.

Bob
__________________
Chevrolet Blitz Half-Track Replica - Finished and Running
Ford F15 - unrestored
Ford F15A X 2 - unrestored
Website owner - salesmanbob.com
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 17:43.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016