			#1  
			
			
			
			
			
		 | |||
| 
 | |||
|  Carrier track link heat treatment 
			
			I hope the attachment on the carrier track link heat treatment, turns out. It may help answer the question were they or weren`t they. Doug | 
| 
			 
			#2  
			
			
			
			
			
		 | ||||
| 
 | ||||
|   
			
			Carrier track is steel.  If steel isn't heat treated after casting it is as brittle as Cast Iron.  Widmanstatten alpha.... ah.. I didn't forget everything they tought me then   Not 100% true, quite early on in he war, if not just before they switched from Manganese Steel to SG, I had forgotton that. 
				__________________ Alastair Lincoln, UK. Under Restoration: 1944 No2 MK2 Loyd Carrier - Tracked Towing 1944 Ford WOT6 Lorry The Loyd on Facebook Last edited by ajmac; 18-10-10 at 23:50. | 
|  | 
| 
 | 
 |