Cadmium Plating is still commonly used in the aircraft industry as a protective coating. A good electroplater will have access to this.

You will find most industrial plating places & hardchrome platers can Cad. Plate. Hardchrome is the kind you see on shock absorber shafts, hydraulic actuators and the like.

Cad plating is muuuuch cheaper than chrome plating.(Not much on a CMP chromed except the wiper arm knob ) Remember to wash you hands if you have touched cadmium plating. It is toxic, and the oxide (looks like salt) is highly toxic.

Ian
__________________
Ian Williams

F15A,
2x Army Land Rover 88' sIIA's
GPW
Other stuff
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 09:28.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016