Molassas do work very well however over a longer period of time, circa two weeks for larger items. Coca Cola contains citric acid which does clean. You can make a vat with 3 %citric acid and soak the item you then have to take it out after 24hours wire brush it then soak for another 24 hours, then wirebrush / jet wash the oxidised waste from the metal. it works well but you have to really flush he steel properly then use a heat gun or blow torch to heat the metal and thoroughly dry it out otherwise it oxidises very quickly.

here is a good demo of this process

http://www.youtube.com/watch?v=ckdMdiJlV7c

and likewise a good example of results from an electrolysis bath for large items... this one is four parts and the link i have put is part four

http://www.youtube.com/watch?v=35nmK...D41B7&index=18
__________________
is mos redintegro

__5th Div___46th Div__
1942 Ford Universal Carrier No.3 MkI*
Lower Hull No. 10131
War Department CT54508 (SOLD)
1944 Ford Universal Carrier MkII* (under restoration).
1944 Morris C8 radio body (under restoration).
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 15:14.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016