#28
|
|||
|
|||
![]()
Hi Tony
"So it is spot on. What I am a bit ticked off about is the semi gloss finish 'cause we also worked on getting a flat to matt finish. The spec's sent to the paint maker specified that 20% flattening agent was required. Anyway I'll work on that." Whose paint did you use? Did you add any hardener or other additive other than the flatten-er? Did you get all the mixture numbers so it can be reproduced? Reason I ask is did a similar process on my HUP and the finial coat just did not flatten the way I wanted. The problems in my case are technique and adding hardener to Enamel. Cheers Phil
__________________
Phil Waterman `41 C60L Pattern 12 `42 C60S Radio Pattern 13 `45 HUP http://canadianmilitarypattern.com/ New e-mail Philip@canadianmilitarypattern.com |
|
|