Default filler

Depending upon the degree of pitting that you have, there is a product here in Canada which is commonly used called hi-fill or hi-solids primer. The intent of this product is to build up thickness, almost a spray Bondo if you will, that is very easy to sand and can almost be "run" to fill in imperfections. It can be applied at a very heavy rate and is very good. It can be applied in several layers to get what you need.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 17:36.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016