Looks Great Matt well done . When I painted the Green I used a small flat brush and cut in around all the hardware e.g. floor fittings, inside dash cut out,
underneath engine rails , also I gave a good coating along all the seams inside the hull , this way when your spraying the big flat panels your not trying to get coverage around things in hard to get places . best to paint up under the drivers compartment first , then fire wall behind you , lower inside walls , floor then panniers then work your way out . Second coat you can take your time and spray away .. I think I used about 25 litres of KG green enamel , 20 litres of primer 1 x 20 litres of enamel thinners 1 x 20 GP thinners best to buy thinners in 20 litres with tap . These numbers are for the complete carrier not just the hull . hope this helps . Dale
__________________
1944 GPW and Bantam trailer
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Similar Threads
Thread Thread Starter Forum Replies Last Post
Restoration of Hull 731- Carrier, MG (Aust) Mortar Carrying Darrin Wright The Restoration Forum 359 25-04-15 07:30
Carrier hull Mick Sutherland The Carrier Forum 1 17-07-13 20:33
Hull # gary_bath_jr The Carrier Forum 5 12-07-10 21:31
Welded hull martyn The Carrier Forum 14 15-03-10 14:02
UC Hull Richard Coutts-Smith The Carrier Forum 14 08-04-08 02:25


All times are GMT +2. The time now is 23:52.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016