Default Hair Dryer

David,

I had the same problem this past winter. I was attempting to 'freshen up' the Carrier and needed matte paint. I was able to get into TSC (selected stores) and get flat tremclad in brown, white, and black.

I could not find yellow in matte so I was standing at a Home Hardware when the paint guy tried to help me. He listened to my story and asked if the work was inside where I could get to it with a hair dryer. I must have given him the "... and what freakin' difference would that make" look as he explained that if you spary the semi gloss paint products then get the hair dryer on them before the stuff dries it makes them quite a bit less glossy. Maybe the gloss is related to the VOCs in the paint that the warm air flashes off...??

I tried it and it worked well enough for me - especially since I have only found flat yellow in the 1/10 oz. sizes at the plastic model shops.

Good luck.


Stewart
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 19:00.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016