Quote:
Originally Posted by Ralph Volkert View Post
...

Caution about using alloys and or stainless steel as sacrificial anode... The alloys such as chromium and other materials are released into the solution
These metals are extremely toxic and extreme care should be used when handling. ESPECIALLY if you are reusing the caustic solution. and allowing the waste metals to accumulate. Do not just throw this solution away in your yard or down the drain. Using just mild steel or an inert material will not create a toxic solution. It will remain just water with caustic pH.
I've read this thread end to end and find the chemistry of the simplest things fascinating. But, I read all these chemicals and acids and solutions mentioned without much discussion of disposal. Bob warned about splashing your clothes, hands and eyes. Another fellow damn near blew himself up with a hydrogen gas arc! So, what happens to the immersion bath after the part is clean? Do you guys pour it out on the ground, down a sewer or neutralize it with the opposing Ph agent? Inquiring minds want to know.
__________________
Terry Warner

- 74-????? M151A2
- 70-08876 M38A1
- 53-71233 M100CDN trailer

Beware! The Green Disease walks among us!
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 21:43.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016